dc.description.abstractTi-6Al-4V material is generally used in biomaterial applications. However, this material is difficult to supply and an expensive material. Instead of Ti-6Al-4V material; It is investigated whether the use of 316 L material as an alternative is easier and more economical. In this study, Ti-6Al-4V and AISI 316 L test specimens made of the material subjected to the test under the same conditions wear performance were investigated using the ball on disc experimental setup. The experiments were carried out in three replicates in a dry and liquid medium. As a result, in the experiments; AISI 316 L samples are coated with PVD method compared to other samples in wear rates and abrasive wear marks on the surface of the samples were found to decrease. In studies using sodium hyaluronate fluid, it was found that the rate of abrasion and wear traces decreased compared to the dry environment. It was determined that 316 L samples coated with PVD method showed better wear performance compared to uncoated Ti-6Al-4V material.
dc.description.abstractTi-6Al-4V material is generally used in biomaterial applications. However, this material is difficult to supply and an expensive material. Instead of Ti-6Al-4V material; It is investigated whether the use of 316 L material as an alternative is easier and more economical. In this study, Ti-6Al-4V and AISI 316 L test specimens made of the material subjected to the test under the same conditions wear performance were investigated using the ball on disc experimental setup. The experiments were carried out in three replicates in a dry and liquid medium. As a result, in the experiments; AISI 316 L samples are coated with PVD method compared to other samples in wear rates and abrasive wear marks on the surface of the samples were found to decrease. In studies using sodium hyaluronate fluid, it was found that the rate of abrasion and wear traces decreased compared to the dry environment. It was determined that 316 L samples coated with PVD method showed better wear performance compared to uncoated Ti-6Al-4V material. Considering the density differences of Ti6Al4V and 316L materials, 316L can be used instead of Ti6Al4V material.
dc.language.isoengen_US
dc.publisherDicle Üniversitesi
dc.relation.ispartofDicle Üniversitesi Mühendislik Fakültesi Mühendislik Dergisien_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectBiomaterialsen_US
dc.subjectTi-6Al-4Ven_US
dc.subjectAISI 316en_US
dc.subjectcoatingen_US
dc.subjectwearen_US
dc.subjecttemperatureen_US
dc.subjectSEMen_US
dc.subjectball on discen_US
dc.titleInvestigation of wear behavior of Ti-6Al-4V and AISI 316 L biomaterials with ball on disc test deviceen_US
dc.title.alternativeTi-6Al-4V ve AISI 316 L biyomalzemelerin aşınma davranışlarının bilye disk deney düzeneği ile araştırılmasıen_US
dc.typearticleen_US
dc.departmentAmasya Üniversitesien_US
dc.identifier.volume11en_US
dc.identifier.issue2en_US
dc.identifier.startpage635en_US
dc.identifier.endpage646en_US
dc.relation.publicationcategoryMakale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.identifier.doi10.24012/dumf.630224
dc.identifier.doihttps://doi.org/10.24012/dumf.630224
dc.department-tempAMASYA ÜNİVERSİTESİ, AMASYA TEKNİK BİLİMLER MESLEK YÜKSEKOKULU, 0000-0002-9033-309X, Türkiye -- SELCUK UNIVERSITY, 0000-0003-2894-1809, Türkiye -- SELÇUK ÜNİVERSİTESİ, 0000-0002-7016-6888en_US
dc.snmzKA_DergiPark_20250327


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster